A. J. Torroba, O. Koeser, L. Calba, L. Maestro, E. Carreno-Morelli, M. Rahimian, S. Milenkovic, I. Sabirov, J. LLorca. Investment casting of nozzle guide vanes from Ni-based superalloys: Part I – Thermal calibration and porosity prediction. Integrating Materials and Manufacturing Innovation 3, 25, 2014. DOI: 10.1186/s40192-014-0025-5