Funding: Industria de Turbopropulsores S.A.
Region: Spain
Project period: 2017 – 2019
Principal Investigator: Dr. Javier Segurado (javier.segurado@imdea.org)
The MICROMECH II project is the follow up of the Clean Sky MICROMECH project and is focused on the development of more elaborated micromechanical models for Inconel 718 alloy (casted and forged).